Construction
|
Use Cases
|
Product name
|
Tickness(mm)
|
Advantages
|
|
Aramid fabrics / Fluoro-erastomer
|
FPC
|
Z500
|
1.0 |
Smooth rubber surface Follow the small bumps Cloth surface is difficult to stick to when heated and pressurized Bendable Siloxane-free |
| S-200 |
2.0 |
| Z165 |
2.3 |
| Fluoro-erastomer / Fluoro-erastomer |
FPC FPD(LCD) |
FX050 |
0.5 |
High compressive displacement retention even after repeated use Smooth rubber surface Follow the small bumps Less contamination Bendable Good sucker absorption, Automatic transfar is possible Siloxane-free |
| Z723 |
1.0 |
| F-200 |
2.0 |
| Aramid fabrics / Aramid fabrics |
PCB Decorative laminated sheet Cards |
R-055 |
0.55 |
Cloth surface is difficult to stick to when heated and pressurized Bendable Difficult to spread during compression Siloxane-free |
| R-075 |
0.75 |
| R-105 |
1.05 |
| R-225 |
2.25 |
| Z497 |
2.3 |
| R-250 |
2.5 |
Aramid fabrics / Aramid fabrics (Antistatic) |
Electronic Devices Building Materials |
G-1 |
1.6 |
High compressive displacement retention even after repeated use Cloth surface is difficult to stick to when heated and pressurized Less electrification during peeling Board-shaped Good sucker absorption, Automatic transfar is possible Siloxane-free |
| G-2 |
2.9 |
| G-3 |
4.2 |
| GA-1 |
2.25 |
Cloth surface is difficult to stick to when heated and pressurized Less electrification during peeling Bendable Siloxane-free |
| GA-2 |
3.4 |